Hi Shankar,

7010-G available with Bohler Welding .They stock it in India and approved by some major Piping contractors.

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Suresh
Sent: Friday, December 31, 2010 10:39 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:9035] Technical solution

 

Hii Sankar ,

 

Plz check below quote from D&H  in India , E 7010 Electrode is available in Indian Market . you  can choose it .

 

 

D&H Secheron through well-built hard work in research and development will meet the various demands of our customers. Below please find a category wise kisting of our latest products.

 

SMAW / MMAW Electrodes

Mild Steel Electrodes

PRODUCT NAME

AWS CODE

IS CODE

 

CELLUTHERME - Mo

E7010-G

E7070-G

 

On Thu, Dec 30, 2010 at 6:23 PM, pradip kumar sil <pradipsil@gmail.com> wrote:

Dear All,

When we use GTAW , we are using  ER-70S2/E-7018( Same tensile) combination, alternatively in SMAW , we are using E-6010/E-7018( Different tensile) instead of E-7010. E-7010 is not available(as per ASME) in the market. Is there any technical problem to manufacture it or to  use it.

Can somebody tell it.

Regards

Pradip

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.




--
Thanks  & Best Regards,

Suresh

Mobile No: 91-92 92 905 905

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...