Hi Elumali,

Thanks for quick feedback.

Yes, it is corrosion test and being done at laboratory having appropriate set up. But the question is that project specification requires it as per ASTM  G 36 ,with cacl2 solution.

Request to provide more information, if available.
regards,
jignesh rana


----- Original Message -----
From: Sundaram Elumalai
To: materials-welding@googlegroups.com
Sent: Thu, 30 Dec 2010 17:06:10 +0530 (IST)
Subject: [MW:9021] RE: 9018] Stress Corrosion Cracking Test


















Hi,



 



This is one corrosion test need to be done
at approved Lab. So you may check in your region, who is doing this test.



 





With Kind regards,



 



S.Elumalai.














From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of jignesh.rana@Linde-LE.com

Sent: Thursday, December 30, 2010
1:45 PM

To: 'materials-welding@googlegroups.com'

Subject: [MW:9018] Stress
Corrosion Cracking Test





 





Dear Members,



One
of our project specification calls for Chloride Stress Corrosion Cracking as
the ASTM G 36 with CaCl2 (40%) solution for super Duplex Stainless steel ( S
32750)




ASTM
G- 36 is based on MgCl2 solution.




Does
any one having experience with SCCT with CaCl2 solution ?




With
Best Regards,



Jignesh R Rana

Manager - QA & QC



Linde Engineering India Pvt. Ltd.

38, Nutan Bharat Society, Alkapuri, Vadodara 390007, India

Tel.: +91 265 3056789, Fax: +91 265 2335213 , Mobil:  +91 90999 86019

jignesh.rana@linde-le.com, www.linde-india.com



This e-mail is confidential. If you are not the intended recipient, please
notify us immediately. You should not disclose its contents to any other person
nor use it for any purposes.





--

To post to this group, send email to materials-welding@googlegroups.com

To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com

For more options, visit this group's bolg at http://materials-welding.blogspot.com/

The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions w.r.t.
applicable code/standard/contract documents.











--

To post to this group, send email to materials-welding@googlegroups.com

To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com

For more options, visit this group's bolg at http://materials-welding.blogspot.com/

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...