Re: [MW:9024] Stress Corrosion Cracking Test

Dear Rana,
                  The test method G36 asks for MgCl2 but it can be done with CaCl2 as per your client spec; basically its the Chloride ion which plays the role in SCC by preferentially attacking the stressed area. Test method is standard but can always be substituted as per our requirements.

2010/12/30 <jignesh.rana@linde-le.com>

Dear Members,

One of our project specification calls for Chloride Stress Corrosion Cracking as the ASTM G 36 with CaCl2 (40%) solution for super Duplex Stainless steel ( S 32750)

ASTM G- 36 is based on MgCl2 solution.

Does any one having experience with SCCT with CaCl2 solution ?

With Best Regards,

Jignesh R Rana
Manager - QA & QC

Linde Engineering India Pvt. Ltd.
38, Nutan Bharat Society, Alkapuri, Vadodara 390007, India
Tel.: +91 265 3056789, Fax: +91 265 2335213 , Mobil:  +91 90999 86019
jignesh.rana@linde-le.com, www.linde-india.com

This e-mail is confidential. If you are not the intended recipient, please notify us immediately. You should not disclose its contents to any other person nor use it for any purposes.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
regards,
Harish.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...