Dear Sir,
             Please refer this site http://www.brertechnical.com/

2010/12/27 Eng/ Mostafa Kamel Hussein <mkh_200@yahoo.com>

Dear sir,

I have fiberglass pipe lines and i want to check the damages for this pipes in order to replace the damaged piping are there any tools or equipments can help me to detect the damages or any other ways?

Regards,

    

Eng/ Mostafa Kamel Hussein

QA/QC manager

SIEMENS Limited,Industrial Solution&Services

Mohandessin - Giza - Egypt

+20104410009

                              

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
regards,
Harish.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...