ASME  B31.1B-2006  Says

 

137.4.5 Required Hydrostatic Test Pressure. The

hydrostatic test pressure at any point in the piping system

shall not be less than 1.5 times the design pressure,

but shall not exceed the maximum allowable test pressure

of any nonisolated components, such as vessels,

pumps, or valves, nor shall it exceed the limits imposed

by para. 102.3.3(B). The pressure shall be continuously

maintained for a minimum time of 10 minutes and may

then be reduced to the design pressure and held for such -    (This time depends upon project requirement- Max 2 hrs)

time as may be necessary to conduct the examinations   

for leakage. Examinations for leakage shall be made of

all joints and connections. The piping system, exclusive

of possible localized instances at pump or valve packing,

shall show no visual evidence of weeping or leaking


 

With regards

  

T.Mahendran,
Tabouk - KSA,
Ph: 059 3423 767.

 
 

From: SOHAIB GHNAIMAT <sohaib_cegco@yahoo.com>
To: materials-welding@googlegroups.com
Sent: Sun, December 26, 2010 9:17:20 PM
Subject: Re: [MW:8951] Hydrostatic Test


Dear Larry , usually the holding time for buried Piping should be 2 hours for the strength test and 24 hours for tightness test , while for above ground piping the holding time should be 30 minutes to two hours ( Depends on project Inspection ) providing that ALL welds should be accessible for visual inspection to any leak.

Regards,

Sohaib   


From: Larry <quality@unieng.com.au>
To: materials-welding@googlegroups.com
Sent: Wed, December 8, 2010 4:18:47 PM
Subject: [MW:8611] Hydrostatic Test

Hi There,

 

Is there any table on holding time on hydrostatic test as per ASME B31.3 NFS, or any table in ASME code that would refer to it?

 

Thanks in advance.

 

Larry Zarate

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35737] Bend Test and Tensile Test failed for ET45 Micro Welded Coupon

Hi As its %elongation is very low  Better try buttering on jt surrace with ductile consumable like pure Ni i. E Ni1 And later weld jt with c...