Resistance to pitting corossion
Sent from BlackBerry® on Airtel

-----Original Message-----
From: Shiv Dutt Mishra Mishra <gopu301182@gmail.com>
Sender: materials-welding@googlegroups.com
Date: Tue, 30 Nov 2010 15:58:07
To: <materials-welding@googlegroups.com>
Reply-To: materials-welding@googlegroups.com
Subject: [MW:8445] Importance of "MO" content in SS316L material.

Dear All,
Can you tell me what is the importance of '' MO"(molybdenum) content
in SS316L materials.

--
Thanks,
S.D.Mishra
Mob- 09589444897 (M.P./C.G.)
09766916581 (Maharastra)

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35742] PQR- Chemical testing requirements

Good Day to all, Reference std: ASME SEX IX Material ASTM A106 Gr B Pipe Dia and thickness: 2" and 8.74 mm. Service Fluid: Normal fluid...