Please give me your view on below query;-

PQR qualified in accordance with ASME sec ix, a fillet weld between dissimilar base metal thicknesses of 25mm and 12 mm, Impact test mandatory,Construction code is ASME sec viii div 1.
 
Since groove weld qualifies for all fillet weld thickness (QW-451.4), does that mean QW-403.6 will not be applicable in this case? i am aware that QW-451.1 is applicable but please let me know regarding QW-403.6.

Awaiting your valuable response.

Regards
Manpreet Singh


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...