Saturday, November 27, 2010

Re: [MW:8397] SS 304 to SS 321 welding

Dear Hrishi
 
 
you need to weld with ER308L / ER308L-15 Electrodes.
 
 
Regards
 
Durai Murugan
QC Welding Inspector


From: "hrishikm07@gmail.com" <hrishikm07@gmail.com>
To: Materials Welding <materials-welding@googlegroups.com>
Sent: Thu, November 25, 2010 4:15:58 PM
Subject: [MW:8385] SS 304 to SS 321 welding

1.Pl advise if SS 304 to SS 321 piping welding is possible? If so what is the consumable to be used
2. Is welding of SS 321 possible with E 308 consumable provided one has an approved WPS/PQR?

Thanks
Hrishi
Sent on my BlackBerry® from Vodafone

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...