Re: [MW:6655] How to protect Serration of Flanges during Hot dip galvanization


Molycoat

is the high temperature grease which can withstand beyond 900 deg C. Check with supplier / manufacturer to use the same for your said application.

l am not sure but I hope it will serve your purpose

Regards..

On 23 August 2010 12:38, aly mhaskar <mhaskar_aly@yahoo.com> wrote:
Dear All,
Presently we are doing hot dip galvanization of pipe spools where we have to protect the serration of flanges during galvanization.
 
Can any body suggest what can be applied on serration to protect it from adhesion of ZINC on serration.
 
Thank you in advance.
 
Mhaskar Aly
Kuwait


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...