Re: [MW:6235] Welder Qualification-Thickness range

If u qualify a welder with above 13 with minimum 3 layers, he is qualified for " max to be welded". if u have joint of maxmum 250 mm in ur shop he is eligible to weld this joint
KGP

On Wed, Jul 28, 2010 at 10:33 PM, naveen <dnkuit@gmail.com> wrote:
Can you explain in detail regarding in SEC IX - QW452.2?
Welder thickness range for unlimited thickness?we are confused?With
example please?

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35346] Cast-iron welding

Any advice for cast iron welding Sent from Yahoo Mail for iPhone