Sunday, August 1, 2010

Re: [MW:6236] why plsama cutting in ss

when u are heating, oxides forms. Oxy-acet has a Kindling temp of 1200 celcius. If any oxides after haeting exceeds this temp can not be cut by oxy-ace flamme
KGP

On Tue, Jul 27, 2010 at 7:10 PM, mijin <mathew.mijin@gmail.com> wrote:
why we are using plasma cutting in stainless steel instead of
oxyacetelene cuttng.please give me a reason...

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...