There should be no Problem using E309Mo below 300 degee centigrade, for metal SS316 to ASTM A106 Gr.B.
 Regards
 Chitturi
 On Wed, Dec 30, 2009 at 7:28 PM, babu k <kbabupsg@gmail.com> wrote:
 
Hi gents,On the basis of metallurgical point of view, is there any effect of choosing E309Mo as the filler metal for the above combination of base metal.Service temp is minus 40 (Max.)Regards,K.Babu,Singapore--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments