Re: [MW:3918] the substitute NDT

you can have RT but for it you have to use strong curie try for it i have tried for SHell of 78mm and it works but in it i use double films for excellent film contrast( ASME INSPECTOR ALLOW ME TO ADOPT THIS METHOD)
if you not want RT then UT too has permanent record or go for TOFD (NEW FORM OF UT)

On Wed, Dec 30, 2009 at 2:55 PM, Eng/ Mostafa Kamel Hussein <mkh_200@yahoo.com> wrote:

I have material with 80mm thickness and it's known that RT is not applicable for application as NDT, so what is the substitute method for NDT and please give me the code case number for that?

Note1: the applied code ia ASME VIII Div II

Note2: If the substitute NDT is UT with permanent record but also it's difficult to get it what is substitute to get NDT with permanent record????

 

Eng/Mostafa Kamel

Senior Welding Engineer

SIEMENS

+20104410009


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
with Regards


SAQIB JALAL
Inspection Engineer
PakArab Fertilizer Limited
Khanewal Road , Multan
office number +92-61-9061 EXT 3110
mobile number +92-321-4043556

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...