Sunday, December 27, 2009

Re: [MW:3908] A312 TP316 SCH 10S WELDING DIA 10"

HI, Try Before You TEST THE WELDERS IN 6G POSITION, GTAW PROCESS AND SPECIMEN of equal diameter, thickness AND MATERIAL, PERFORM VISUAL AND MECHANICAL TESTS O RADIOGRAPHIC TEST OF SPECIMEN.

 

GOOD LUCK

 

AGUSTIN JIMENEZ




De: "george.dilintas@gr.bureauveritas.com" <george.dilintas@gr.bureauveritas.com>
Para: materials-welding <materials-welding@googlegroups.com>
Enviado: sáb, diciembre 26, 2009 1:46:42 PM
Asunto: Re: [MW:3903] A312 TP316 SCH 10S WELDING DIA 10"

GTAW process with gas bucking.


  From: "ramesh  p" [withuramz@rediffmail.com]
  Sent: 26/12/2009 17:07 GMT
  To: <materials-welding@googlegroups.com>
  Subject: [MW:3902] A312 TP316 SCH 10S WELDING DIA 10"


Dear Friends,Seniors,
Subject:-A312 TP 316L SS, SCH 10S WELDING,DIA 10"
We are facing too many failures with our welders in Welding of SS Sch 10S (Lower Thickness).Even Good welders are not able to give good penetration even with adequate purging.Fusion is not clear.Sometimes the shape changes.
Is it bcoz of the ability of the Welder only or Something extra need to be taken care ?
Anybody can give me useful tips/suggestions to come over this issue? Any useful tips to the welders?
Warm Regards
Ramesh
QA/QC Engineer
Galfar Al Misnad Engg & Contg.W.L.L
Doha-QATAR


THIS IS YOUR DAY..YOU CAN..YES..DO IT...


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



¡Obtén la mejor experiencia en la web!
Descarga gratis el nuevo Internet Explorer 8
http://downloads.yahoo.com/ieak8/?l=e1

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...