Tuesday, December 22, 2009

Re: [MW:3871] Filler wire & Electrde Req.

Dear Prashant,
 
Please note that you can used ER 4043, as we hve used in our previous company for making aluminium duct for RIL.

ER1100 is suitable, but ER 4043 may be used for some applications. refer SFA 5.10 for selection choice.
 
shabbir
 
On 12/21/09, prashant pansare <prashantpan_99@yahoo.co.in> wrote:
Dear All,
I' ve to weld SB 290 ALUMINIUM 1100, I m using ER 4043,but I m not sure weather it's a pefect filler wire.
Is there any chart available to choose appropriate filler wire or electrode  for the perticular material?
Pl. forward.
Thanx in advance & Merry X' mas to all of u.
PSP  


The INTERNET now has a personality. YOURS! See your Yahoo! Homepage.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...