Re: [MW:3868] Clarification on range of qualification as per AWS D1.1



On Mon, Dec 21, 2009 at 2:32 PM, Sankepalli R.S.Reddy <sankepalli.rsreddy@gmail.com> wrote:
Dear Members,
 
I have a query related to welder qualification for TKY joints as per Table 4.11 and Fig 4.27 - AWS D1.1
 
1. Can we use a pipe with thickness less than 12mm or 0.5" during welder qualification. What is the minimum thickness allowed per code.
 (Since the specified thickness is nominal, may i use a pipe with thickness less upto 12.5% - Material SA 106 GrB)
(Look at the figure 4.27 , minimum wall thickness is 12 mm)  
 
2. If welder is qualified in Group 1, can he weld Group 2 & 3
(AWS Group is not essential variable , so if u qualify the group I, will qualify the all groups)
.
 
 
 
Thanks and regards
 
S. Rama subba reddy
Offshore/Onshore Inspection group
Saudi Aramco

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



Thanks & regards,

K.Babu
Singapore

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...