Wednesday, December 30, 2009

Re: [Bulk] [MW:3926] WPS & PQR clarification

In simple words in construction language I can explain WPS / PQR as follows....

there will be Drawing approved for Construction = WPS prepared in initial stage
Construction process as per approved Drawing = Qualifiying PQR and Testing
As built Preparation and using the approved drawing for Proto type items = Modified WPS based on PQR data, used during welding of similar welds in future

Hope I made it clear....

Regards.
C. K. Purohit
Eng-Tech Weld1
Sr Welding Inspector


2009/12/30 mahen dran <cbemahendar@yahoo.com>
Dear Group
 
 Good day,
--------------------------------------------------------------------------------------------------------------------------------
Still I have confusion on WPS and PQR terms.
 
1. WPS to be created  first , with respect to  selection of process, electrode and current  etc.
2. PQR is developed  after WPS ,by entering the the actual variation  relevant to the WPS.
 
|Corresponding reference numbers are to be entered  in each other.
 
This is the information  from ASME IX codes.
 --------------------------------------------------------------------------------------------------------------------------
But there is a controvercial  statement  from some of our colleques, PQR to be developed first and  Supporiting PQR  reference number is to be entered in the WPS.
 
Please clarify this confusion .
 
 
mahendra
KSA

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...