Thursday, December 31, 2009

[MW:3931] RE: 3928] Welder Qualification

Yes, you can send for RT and Bend test. We have done so many welders qualification under this specification and faced few problems like below.

 

Note: This situation is bit different from ASME Sec IX QW 306 in which the weld metal is deposited by the welder or welders by pass/layer over another pass/layer. Whereas, the below situation is entirely different. We have convinced PDO to proceed further.

 

 

Regards,
Vasanth


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of roshan shan
Sent: 31 December 2009 07:22
To: materials-welding@googlegroups.com
Subject: [MW:3928] Welder Qualification

 

Dear all,

 

Here we have a situation,

 

1) welder qualification conducted on 24" pipe as per Sec IX and client requirement(PDO SP-1096) with two welders welding from opposite sides( one welder welds the half portion and the other half by another welder).

2) RT accepted for 1st half of the portion, but the other half fails to meet the requirement.

 

Question: Whether the test coupon shall be sent for bend testing to qualify the welder who welded the first half?

 

 

NB:RT & Bend test required as per Client requirement.

 

Regards

 

Roshan

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


*** WORLEYPARSONS GROUP NOTICE *** "This email is confidential. If you are not the intended recipient, you must not disclose or use the information contained in it. If you have received this email in error, please notify us immediately by return email and delete the email and any attachments. Any personal views or opinions expressed by the writer may not necessarily reflect the views or opinions of any company in the WorleyParsons Group of Companies."

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...