Here we have a situation,
 
1) welder qualification conducted on 24" pipe as per Sec IX and client requirement(PDO SP-1096) with two welders welding from opposite sides( one welder welds the half portion and the other half by another welder).
2) RT accepted for 1st half of the portion, but the other half fails to meet the requirement.
 
Question: Whether the test coupon shall be sent for bend testing to qualify the welder who welded the first half?
 
 
NB:RT & Bend test required as per Client requirement.
 
Regards
 
Roshan

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...