Skip to main content

[MW:1973] Re: WELDER QUALIFICATION

Dear all,

I would like to add a point here. So far as I understand, you need to use a
qualified procedure for welded qualification as well (Refer QW 301.2). In
this situation, you cannot use any hypothetical WPS (like, P1#P1/F5) unless
otherwise you qualify the same accordingly. I remember we had qualified
such procedure once and for all when I was WE at L&T Hazira Works.

Best regards,

Prasad



BHARAT GOLE
<bharatgole@hotma
il.com> To
Sent by: material welding
materials-welding <materials-welding@googlegroups.com
@googlegroups.com >
cc

17/04/09 10:18 AM Subject
[MW:1971] Re: WELDER QUALIFICATION

Please respond to
materials-welding
@googlegroups.com


Mr. Dale Jones
As you said to weld with F5 stainless steel filler material which is needed
to weld with matching filler on P8 materials.I would like to add
more...i.e. as per QW 423 Alternate Base Materials for welder qualification
we can weld P1 materiel also with F5 SS Filler in order to qualify welder
for any particular P8 WPS.
This is economical as well as within limit of code.
Please correct me if my interpretation is wrong
Regards

Bharat B. Gole


Date: Thu, 16 Apr 2009 16:26:34 -0700
From: dalejones7978@yahoo.com
Subject: [MW:1970] Re: WELDER QUALIFICATION
To: materials-welding@googlegroups.com

This is correct that the welder can weld on all of these materials but do
not ignore the other variables. For example the welder will be restricted
to the Fnumber filler material he qualified with. An example is a SMAW
qualification. When a welder qualifies on P1 material with a matching F4
SMAW filler he will be qualified to the base material range stated below
and with F1-F4 carbon steel filler material. This will not qualify him to
weld with F5 stainless steel filler material which is needed to weld with
matching filler on P8 materials. The same concept will apply to various
other P numberd materials. To fully understand this concept and the other
variables that will restrict a welders qualifications, read article 3 and
QW-416 in ASME Section 9

Regards,

Dale Jones

--- On Thu, 4/16/09, Muhammed Ibrahim <ibratech@gmail.com> wrote:

From: Muhammed Ibrahim <ibratech@gmail.com>
Subject: [MW:1968] Re: WELDER QUALIFICATION
To: materials-welding@googlegroups.com
Date: Thursday, April 16, 2009, 5:45 AM



Not only P11. Also P34 & P41 thru P49. The reason is, the skill of the
welder required to weld any of these material is same. So he can proove
it in any one P No. mentioned .

Regards,
Muhammed Ibrahim


2009/4/16 gaurav mongia <er.gauravmongia@gmail.com>

IF A WELDER IS QUALIFIED FOR P1 material and in code it is written
that he is qualified upto P11.

i wanna know what will be reason that a welder can do welding on
all
material upto P11 instead he is only qualified in P1









How fun is this? IMing with Windows Live Messenger just got better.

Save a tree...please don't print this e-mail unless you really need to.

Save a tree...please don't print this e-mail unless you really need to.




This email and any attached files ("Message") may contain confidential and/or privileged information. It is intended solely for the addressee(s). If you receive this Message in error, inform the sender by reply email, delete the Message and destroy any printed copy.
Any unauthorized use, distribution, or copying of this Message or any part thereof is prohibited. Emails are susceptible to alteration. Neither Technip nor any of its affiliates shall be liable for the Message if altered or falsified nor shall they be liable for any damage caused by any virus that might be transmitted with this Message.


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...