Skip to main content

[MW:1970] Re: WELDER QUALIFICATION

This is correct that the welder can weld on all of these materials but do not ignore the other variables. For example the welder will be restricted to the Fnumber filler material he qualified with. An example is a SMAW qualification. When a welder qualifies on P1 material with a matching F4 SMAW filler he will be qualified to the base material range stated below and with F1-F4 carbon steel filler material. This will not qualify him to weld with F5 stainless steel filler material which is needed to weld with matching filler on P8 materials. The same concept will apply to various other P numberd materials. To fully understand this concept and the other variables that will restrict a welders qualifications, read article 3 and QW-416 in ASME Section 9

Regards,

Dale Jones

--- On Thu, 4/16/09, Muhammed Ibrahim <ibratech@gmail.com> wrote:

From: Muhammed Ibrahim <ibratech@gmail.com>
Subject: [MW:1968] Re: WELDER QUALIFICATION
To: materials-welding@googlegroups.com
Date: Thursday, April 16, 2009, 5:45 AM

 
 
Not only P11. Also P34 & P41 thru P49. The reason is, the skill of the welder required to weld any of these material is same. So he can proove it in any one P No. mentioned .
 
Regards,
Muhammed Ibrahim

 
2009/4/16 gaurav mongia <er.gauravmongia@gmail.com>

IF A WELDER IS QUALIFIED FOR P1 material and in code it is written
that he is qualified upto P11.

i wanna know what will be reason that a welder can do welding on all
material upto P11 instead he is only qualified in P1








--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Re: [MW:14950] RE: 14919] Stress relieving Rejected for 5 min less soaking time.

Dear All, I have been a CONSULTANT FOR such problem & my personal opinion is expressed as follow. I fully agree with views expressed so far. But bag to differ that " Code is a law, with engineering judgments. Hence the inspector has the rights to declare that the original HT was inadequate." Inspectors & total industry must resist the "REJECTION" . We as intellectual & having seniority must become practical. How the code will revise???. ANS.: One is experiments (Pure research) & second is such chances that gives opportunity to experiment !!! _______________________________________________________________________________________________ My understanding is that it is P1 material. In that case every pass normalizes the immediate bottom pass. Hence code requirement for P1 FOR MANDATORY SR is 32 mm & above thickness. SOLUTION:  In any case 0. After SR=PWHT no PTC testing is required as per code--Unless for low temp. vessels. That means code ...