Tuesday, November 11, 2008

[MW:1287] Re: Impact testing values

If your question is regarding acceptable value, same value/energy must be
for parent/ HAZ/Weld metal for a particular application/design..
If your question is whether value will be similar, No. Normally impact
values will be relatively lowest for the specimen than taken from weld
centre (As welded). When you compare the order will be Weld centre (lowest),
HAZ area, Parent Metal. (unaffected by welding).
Regards,
Sanjeevan

----- Original Message -----
From: <Sudipto_Banerjee@fwuk.fwc.com>
To: <materials-welding@googlegroups.com>
Sent: Monday, November 10, 2008 6:36 PM
Subject: [MW:1281] Impact testing values


>
> Can anyone tell me whether the impact test value will be same for the
> parent metal and the weld metal? or it can be different.
>
> Best Regards,
> Sudipto Banerjee
> Man. no. B 4974
> Equipment Engg. Department
> Office no. 0044- (0)118 913 2295
>
>
> =======================================================
> Confidentiality Notice
>
> This communication and the information it contains:-
> (a) Is intended for the person(s) or organisation(s) named above and for
> no other person(s) or organisation(s).
> (b) May be confidential, legally privileged and protected in law.
> Unauthorised use, copying or disclosure of any of it may be unlawful. If
> you have received this communication in error, please contact us
> immediately by email at Postmaster@fwuk.fwc.com.
> =======================================================
>
>
> >


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...