Thanks.
But if you refer to UG-84 (g)(5) it says it should be at least as high as
the base metal (parent metal).
Best Regards,
Sudipto Banerjee
Man. no. B 4974
Equipment Engg. Department
Office no. 0044- (0)118 913 2295
"Monica Cristina Riccio
Ribeiro"
<MRRIBEIRO@firjan.org.br> To
Sent by: materials-welding@googlegroups.com
materials-welding@googleg cc
roups.com
Subject
[MW:1282] RES: 1281] Impact testing values
10/11/2008 16:45
Please respond to
materials-welding@googleg
roups.com
It is different!!!
-----Mensagem original-----
De: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com]Em nome de
Sudipto_Banerjee@fwuk.fwc.com
Enviada em: segunda-feira, 10 de novembro de 2008 11:37
Para: materials-welding@googlegroups.com
Assunto: [MW:1281] Impact testing values
Can anyone tell me whether the impact test value will be same for the
parent metal and the weld metal? or it can be different.
Best Regards,
Sudipto Banerjee
Man. no. B 4974
Equipment Engg. Department
Office no. 0044- (0)118 913 2295
=======================================================
Confidentiality Notice
This communication and the information it contains:-
(a) Is intended for the person(s) or organisation(s) named above and for no
other person(s) or organisation(s).
(b) May be confidential, legally privileged and protected in law.
Unauthorised use, copying or disclosure of any of it may be unlawful. If
you have received this communication in error, please contact us
immediately by email at Postmaster@fwuk.fwc.com.
=======================================================
"As informações existentes nesta mensagem e nos arquivos anexos são para
uso restrito e confidencial, sendo seu sigilo protegido por lei. Se você a
tiver recebido por engano, por favor, notifique imediatamente ao remetente
e remova a mensagem e qualquer anexo de seu sistema. O Sistema FIRJAN não
se responsabiliza por qualquer omissão ou falhas contidas nesta mensagem,
que possam surgir na transmissão da mesma ou por prejuízos provenientes de
quaisquer alterações de seu conteúdo. Esta mensagem é de responsabilidade
de seu autor e seu conteúdo não reflete, necessariamente, a opinião da
empresa".
=======================================================
Confidentiality Notice
This communication and the information it contains:-
(a) Is intended for the person(s) or organisation(s) named above and for no other person(s) or organisation(s).
(b) May be confidential, legally privileged and protected in law. Unauthorised use, copying or disclosure of any of it may be unlawful. If you have received this communication in error, please contact us immediately by email at Postmaster@fwuk.fwc.com.
=======================================================
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---
Subscribe to:
Post Comments (Atom)
Re: [MW:35686] HDPE WPS
Refer ASME SEC IX There is separate chapter for Plastic welding . Based on that you have to prepare Sent from my iPhone On 21 Jun 2025, at...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-