Dear Friends,
As per our approved WPS says welding electrode 6010 & 7018 make is ESAB, but our welders is not comfortable for ESAB 6010, They confortable to weld Lincoln Make. please advice me it is allow to weld Lincoln Make. if code is saying anything please give the details.
--
--
Thanks and Regards
Prabhu Duraisamy