[MW:9850] Groove design and bevel

 Dear All,

 

I have a query, kindly share your valuable knowledge on this subject.

 

1-As per ASME IX,  Table QW-253 and QW-256, groove design is non-essential variable for SMAW and GTAW welding.

2-As per ASME B31.3, Fig 328.4.2 and ASME B16.25 Fig 3 and 5 (also Para 3.1C), components having thickness above 22 mm shall have compound bevel.

 

I would like to know that if the requirements of ASME B31.3 and 16.25 as stated above are mandatory? Because as per SEC IX, it is non-essential variable.

What I have observed at site, all pipes and fitting above 22 mm thickness have compound bevel from manufacturer, but all bevel prepared at side are single bevel. Is this acceptable?

 


 
Ahmed Husain
Mob-0547170325