Dear Sirs,

We presently have a 316L matl 3/8" wall thk. cyclone separator (F&D
head & cone bottom) that the Client has speced out to API 620 Code.
The operating temp is 215 deg F and design temp is 300 deg F, op
pressure is 3 psig to 5 in. wc vacuum and design pressure is 7.5 psig
to 15 in. wc vacuum.

Test reqs are 10 psig hydro and spot RT w/ 85% jnt efficiency.

API 620 states in 5.26 Radiographic/Ultrasonic Examination
5.26.4.3 (a) When parts of tanks do not require complete
examination, circumferential joints in cylindrical or conical surfaces
need to be prepared and examined for a distance of only 3 in. on each
side of any intersection with a longitudinal joint. All joints in a
spherical, torispherical, or ellipsoidal shape or in any other surface
or double curvature shall be considered longitudinal joints.

Does this mean that ALL "T" type joints (circ.-to-long seams) require
RT?

Appreciate your interpretation and comments,
Robert

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...