ASME SECTION VIII DIV.1
UW-42 SURFACE WELD METAL BUILDUP
Construction in which deposits of weld metal are applied
to the surface of base metal for the purpose of:
(a) restoring the thickness of the base metal for strength
consideration; or
(b) modifying the configuration of weld joints in order
to provide the tapered transition requirements of UW-9(c)
and UW-33(b) shall be performed in accordance with the
following rules:
(1) A butt welding procedure qualification in accordance
with provisions of Section IX must be performed for
the thickness of weld metal deposited, prior to production
welding.
(2) All weld metal buildup must be examined over
the full surface of the deposit by either magnetic particle
examination to the requirements of Appendix 6, or by liquid
penetrant examination to the requirements of Appendix 8.
When such surface weld metal buildup is used in welded
joints which require full or spot radiographic examination,
the weld metal buildup shall be included in the examination.
--
அருணாசலம்
கலைவாணி
சுதர்ஷனா
வருண்
-- UW-42 SURFACE WELD METAL BUILDUP
Construction in which deposits of weld metal are applied
to the surface of base metal for the purpose of:
(a) restoring the thickness of the base metal for strength
consideration; or
(b) modifying the configuration of weld joints in order
to provide the tapered transition requirements of UW-9(c)
and UW-33(b) shall be performed in accordance with the
following rules:
(1) A butt welding procedure qualification in accordance
with provisions of Section IX must be performed for
the thickness of weld metal deposited, prior to production
welding.
(2) All weld metal buildup must be examined over
the full surface of the deposit by either magnetic particle
examination to the requirements of Appendix 6, or by liquid
penetrant examination to the requirements of Appendix 8.
When such surface weld metal buildup is used in welded
joints which require full or spot radiographic examination,
the weld metal buildup shall be included in the examination.
On Thu, Dec 23, 2010 at 11:33 AM, Mani <kumarmani12@gmail.com> wrote:
Dear all,
In pressure vessel fabrication , contractor has repaired the pits area
in shell without getting approval from client.
Without raising NCR what are the steps and ndt activites we can take
against this issue?
Thanks
Mani
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
அருணாசலம்
கலைவாணி
சுதர்ஷனா
வருண்
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments