01.Dimensions and Weights for medium weight pipes to
DIN 2440 and heavy weight pipes to DIN 2441

o2.
DIN flange summary chart
Description Rated Pressure / Presión Nominal / Nenndruck (in bar) (1 bar = 14.5 psi)
  1 2.5 6 10 16 25 40 64 100 160 250 320 400
  DIN
Blind Flanges     2527 2527 2527 2527 2527 2527 2527        
Flat flange for welding (slip-on)     2573 2576                  
Welding neck flanges 2630 2630 2631 2632 2633 2634 2635 2636 2637 2638 2628 2629 2627
Lapped flanges, Plain collars     2641 2642                  
Loose flanges and rings for welding     2652 2653   2655 2656            
Loose flanges and rings with neck for welding       2673                  
Oval plain threaded flanges     2558                    
Oval flanges, with neck threaded       2561 2561                
Threaded flanges with neck     2565 2566 2566 2567 2567 2568 2569        
Long neck welding flanges           28115   28115              
Hubbed slip-on flanges for welding    
86029 86030                

you try the following ..useful to you.
http://mdmetric.com/home3.htm

Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Wed, 12/8/10, Bagesh <bagesh.kmr@gmail.com> wrote:

From: Bagesh <bagesh.kmr@gmail.com>
Subject: [MW:0] DIN Dimensional Code like ASME
To: materials-welding@googlegroups.com
Cc: piping_valves@yahoogroups.com
Date: Wednesday, December 8, 2010, 1:56 PM

Dear All,

         I have struck up for a project of Munich , Would like to get the dimensional code No. Like ASME B16.9 of Wrought Fittings, ASME B16.5 for Flanges, similarly DIN also should have the standard related to the dimensional correctness.

The Material is SS316 Ti, from DIN EN 1.4571

Can I get these Dimensional Standards name, which may be but not limited to ASME equivalent. I need these dimensional standards for Pipes, Fittings (Forged and Wrought SW and BW), Flanges(WN and SW) (Olets if any) etc. I tried to get through Internet, but it seems they are quite confusing there.

Thanking you all in Advance and will appreciate for this help.

 

===================
Bagesh Kumar

Seoul 135985

===================

 

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...