Hi
ist of all please confirm whether it is high grade filler wire or alloy grade filler wire,
yes for Cabon steel, alloy grade such as austenite and Nickel electrodes (23cr : 12 Ni) can be used in order to avoid Hydrogen cracking specially when Preheat is impractical,
The phrase is mostly applicable to C-Mn steels.
Regards
Manpreet Singh
Welding Engineer
On Tue, 07 Dec 2010 22:20:38 +0530 siva chidambaramwrote
>Dear once,
>
>What will happen when welding of carbon steel material with alloy filler wire.
>If so what will be corrective action to be taken
>
>M.Sivachidambaram
>Welding Engineer
> --
>To post to this group, send email to materials-welding@googlegroups.com
>To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
ist of all please confirm whether it is high grade filler wire or alloy grade filler wire,
yes for Cabon steel, alloy grade such as austenite and Nickel electrodes (23cr : 12 Ni) can be used in order to avoid Hydrogen cracking specially when Preheat is impractical,
The phrase is mostly applicable to C-Mn steels.
Regards
Manpreet Singh
Welding Engineer
On Tue, 07 Dec 2010 22:20:38 +0530 siva chidambaram
>Dear once,
>
>What will happen when welding of carbon steel material with alloy filler wire.
>If so what will be corrective action to be taken
>
>M.Sivachidambaram
>Welding Engineer
> --
>To post to this group, send email to materials-welding@googlegroups.com
>To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments