Skip to main content

Re: [MW:8468] Re: RT/UT OF SOCKET WELD/BRANCH WELD

It is also ARAMCO requirement  to take NDT to verify gaps in SW joints.

 

Regards,

AHusain
 



From: Raghuram Bathula <raghurambathula@gmail.com>
To: Materials & Welding <materials-welding@googlegroups.com>
Sent: Wed, December 1, 2010 10:31:11 AM
Subject: [MW:8461] Re: RT/UT OF SOCKET WELD/BRANCH WELD

Yes it is common to check 5% or 10% of welds, but 100% RT as specified
in this stnadard is something strange.

On Dec 1, 11:47 am, "paresh k patel" <pkpatel1...@rediffmail.com>
wrote:
> Dear Jignesh
>
> Hi! How are you? Hope fine.
>
> Yes this is carried out to detect gap. In many companies this practice is adopted to verify gap for SW joints.
>
> Regards
>
> Paresh Patel
> ABS IV
>
> On Wed, 01 Dec 2010 07:17:32 +0530  wrote
>
> >Few days ago i came across UOP specification 8-11-12-Piping, which asked radiography of socket / branch welds for low alloy steel/SS. If somebody has done project with UOP in past, pl share their experience.
>
> Also i read one very old B 31.3 Interpretation: 5-13 for the radiography of socket welds as below...
>
> Subject:ANSI/ASME 831.3-1984 Edition, With the ANSI/ASME 831.3a-1984 Addenda, Table 327.4.1A, Limitations on Imperfections in Welds-Internal Porosity 
> Date Issued: December 2, 1986
> Question (1): In ANSI/ASME 831.3, Table 327.4.1 A, under internal porosity forfillet, socket, seal and reinforcement attachment welds, the wording NA (not applicable) is indicated. Does this mean that radiographic examination is not required for this type of joint configuration?
>
> Reply (1): Yes.
> In my opinion, RT of SW is only performed to detect the gap between two components, also in past during some corossion isometric study, we have assigned TML (thikness monitoring location) to carry out RT of SW/BW to confirm the correctness of welded heavy schedule components.
>
> Can any one write few words about the technical feasibility and effectiveness of final result to confirm the soundness of SW/Branch weld by RT/UT with code back up? If somebody have any digital RT film of SW joint pl share.
>
> Best Regds

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...