Please inform bolts are required for onshore or offshore environment.

 

In offshore environments,

For SS flanges, even SS304 /316 ( due to crevice corrosion problems in corrosive atmosphere ) Bolts are not preferred,

CS Galvanised bolts are any way not preferred due to galvanic corrosion problems ( I think )

 

We use

a. UNS 32760 Bolts or

b. CS/LTCS + Fluropolymer coated bolts (see attachment)

 

Regards,

Shivanand R Ranasaria


From: desaid@toyoindia.com [mailto:desaid@toyoindia.com]
Sent: Friday, December 04, 2009 3:18 PM
To: materials-welding@googlegroups.com
Cc: materials-welding@googlegroups.com
Subject: Re: [MW:3795] type coated Bolts carbon steel bolts ( A193 Gr. B7 ) fo Stainless steel flanges

 


<Security Level 2>                                                                                                                                                                                                                                                                                                                                                                                                                                
Many Licensor's specification specifies A193 B7 / 2H bolts for stainless steel flamges.
Use of galvanised bolt not seen at all for SS flanges.

Also note, A193 B7/2H bolts are not CS bolts. These are alloy steel bolts.

I did not understand the stage of your project . If youare planning to buy new one than buy ss bolts or can go for B16 / 4 bolts also.


Thanks & Regards,
Dhwani Desai.
TOYO - PLANNING & PIPING DEPT.
91-22-2573 7681.


"Pisat, R. R(ahul)" <Rahul.Pisat@akzonobel.com>

12/04/2009 02:33 PM

Please respond to
materials-welding@googlegroups.com

To

<materials-welding@googlegroups.com>

cc

 

Subject

[MW:3787] type coated Bolts carbon steel bolts ( A193 Gr. B7 ) fo         Stainless steel flanges

 

 

 




Hello all,

Please recommend me the type of coated carbon steel bolts ( A193 Gr. B7 ) to use with stainless steel flanges.
I am sure no to apply galvanised bolts with SS flanges.

Our construction team is worried about the rusted of the carbon steel bolts to be apply with stainless steel flanges.

Please reply your recommendation for type of coating for bolts ?

Kind regards

Rahul

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



===================
Please consider the environment before printing this email
===================

The information contained in this communication is intended solely for the use of the individual or entity to whom it is addressed and others authorized to receive it. It may contain confidential or legally privileged information. If you are not the intended recipient you are hereby notified that any disclosure, copying, distribution or taking any action in reliance on the contents of this information is strictly prohibited and may be unlawful. If you have received this communication in error, please notify us immediately by responding to this email and then delete it from your system. NPCC is neither liable for the proper and complete transmission of the information contained in this communication nor for any delay in its receipt.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...