Friday, December 4, 2009

[MW:3790] RE: 3787] type coated Bolts carbon steel bolts ( A193 Gr. B7 ) fo Stainless steel flanges

Most of the client's specs I've seen specify Hot Dip Galvanized bolts to ASTM A153. for both carbon and stainless steel.
 
Unless there is a restriction from a process fluid point of view (i.e. corrosive for galvanized coatings). In that case you may have to investigate other type of bolt materials (A193 B8 - Austenitic Stainless Steel) or other types of coatings.
 
Regards,
 
Gabriel


From: Pisat, R. R(ahul) [mailto:Rahul.Pisat@akzonobel.com]
Sent: 04 December 2009 09:04
To: materials-welding@googlegroups.com
Subject: [MW:3787] type coated Bolts carbon steel bolts ( A193 Gr. B7 ) fo Stainless steel flanges

Hello all,

Please recommend me the type of coated carbon steel bolts ( A193 Gr. B7 ) to use with stainless steel flanges.
I am sure no to apply galvanised bolts with SS flanges.

Our construction team is worried about the rusted of the carbon steel bolts to be apply with stainless steel flanges.

Please reply your recommendation for type of coating for bolts ?


Kind regards

Rahul

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

This e-mail and any attachment are confidential and may be privileged or otherwise protected from disclosure. It is solely intended for the person(s) named above. If you are not the intended recipient, any reading, use, disclosure, copying or distribution of all or parts of this e-mail or associated attachments is strictly prohibited. If you are not an intended recipient, please notify the sender immediately by replying to this message or by telephone and delete this e-mail and any attachments permanently from your system.