Hello experts.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/69834b4e-cf81-4c1a-86b9-49b0d2d9d393n%40googlegroups.com.
Hope all is well.
I want to do welding of NI200 to SS 304 which filler wire I should use for that.
Best regards.
S.K
-- https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/69834b4e-cf81-4c1a-86b9-49b0d2d9d393n%40googlegroups.com.
Comments