Re: [MW:31446] B31.3 PWHT & Preheat Exemption

Yes your Client is correct. Please see the snap shot below.
Inline image

Inline image


Thanks & Regards

J.Gerald Jayakumar




On Monday, 14 September, 2020, 03:02:36 pm GMT+7, Nazeer <naz.mhd@gmail.com> wrote:


Dear All,

Request Clarification on which thickness (Control thickness / Nominal thickness) to be applied in the B31.3 2014 -Table 331.1.3  for PWHT & Preheat exemption. Details furnished below.

Weld Joint Details:
Joint : Header Pipe to Weldolet
Weld Type: Integrally Reinforced Branch Connection (B31.3, Fig 3285.4)
Material: P.No 1
Header Pipe Size: NPS 16 , 12.7mm thick
Weldolet Size: NPS 16 x NPS 3 , sch 40
joint groove Thickness (At crotch of Header pipe & weldolet): 22mm
Nominal Thickness (Tm) As per B31.3, Fig 3285.4 : 22mm
Calculated Control Thickness (Tm+Tc):  28mm (22 + 6mm)

Based on above scenario, we had applied weldolet nominal material thickness Tm of 22mm (thicker member of the joint) on B31.3 Table 331.1.3  and not performed PWHT & preheat of 95 Deg C.

Capture.JPG

Whereas for PWHT exemption, Client is applying the control thickness  of 28mm on B31.3 Table 331.1.3 and insisting us to perform PWHT on the joint due to 95 Deg C preheat not applied.

In my opinion, nominal Thickness to be applied for PWHT exemption and control thickness to applied for calculating Minimum PWHT holding time.

Please advice and enlighten further, whether PWHT is mandatory for the above specified weld joint.


Thanks & Regards
Nazeer





--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/455cdcdb-416f-48ad-abdb-b87c15866e21n%40googlegroups.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...