Skip to main content

Re: [MW:31410] PWHT Thickness Requirements.

Hello Mr. Ghulam,
Yes you can perform PWHT for any P No. even it's exempted as per B 31.3.
For P8 ,yes you can. We advise to perform the PWHT for stabilized SS grades of higher thickness (could be beyond 20 mm ) to avoid the Stress Relaxation cracking. 
But in general it's not required.

Br,
Atul 

On Tue, Sep 8, 2020 at 11:01 AM Ghulam Mustafa <gmt.lah@gmail.com> wrote:
Hello all members,
can we perform PWHT except P1 material.
(such as P8)

Best Regards
GMT


On Tue, Sep 8, 2020 at 9:41 AM atul khatri <atul.mnnit@gmail.com> wrote:
Hello Mr. Andrew,
ASME B31.3 states the general guidelines for PWHT requirements irrespective of fluid service.
Please follow the service specific standards like API RP 941 for Hydrogen service at elevated temperatures , NACE MR0103 etc.
Client requirements may also supersede the code requirement.
Feel free to discuss more.

Thanks & Regards 
Atul Khatri

On Mon, Sep 7, 2020 at 5:22 PM 'james gerald' via Materials & Welding <materials-welding@googlegroups.com> wrote:
There are reasonable changes in ASME B31.3 2018 edition which exempts PWHT if applied a Preheat of 95degC for P1 materials. Please check.

Thanks & Regards

J.Gerald Jayakumar



On Monday, 7 September, 2020, 06:26:18 pm GMT+7, 'Sankaran Sp' via Materials & Welding <materials-welding@googlegroups.com> wrote:


Dear Mr.Andrew,

irrespective of code, for P1 type material with 25mm and above thickness, after pre- heating & welding. PWHT is recommended one and it will reduce the HAZ hardness & eliminating the failure during service.  

Regards,
Sankaran.SP
Welding & Metallurgy expert



On Monday, 31 August, 2020, 07:57:49 pm IST, Andrew Ubakwem <andyubakwem@gmail.com> wrote:


Dear all

Pls what is the current thickness requirements for PWHT as per ASME B31.3? 

I came across old version of the code, it specifies that PWHT not required for all P1 materials, provided min preheat is maintained at 95deg'C.

We intend welding; 18" sch 80(23.83mm) to ASTM A 106, 24" sch 80(30.8mm), is PWHT required? Cite relevant Code sections Please.

Regards,

Andrew. 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAK1J--O6jttEt5bS1QCjykeCFnGeJpwoKsBqPPt9M_P1dOx%3DrA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/624878146.2608697.1599477398043%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/2004183505.3052406.1599479330485%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACKOSeB_KqHyNHmaAgjbTZNgDS%2BEHA3kHr4TnbgcrkRS6z5LCw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHnLYC%2BP3O%3D85auQe_tZGgduMWspaFRF8Qck1GNKSmXBdmvfDA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACKOSeBWYmnOsMV5tCG%2B131QMwDn50Us%2B1ugXC_gPAu_TpZ9_g%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Re: [MW:14950] RE: 14919] Stress relieving Rejected for 5 min less soaking time.

Dear All, I have been a CONSULTANT FOR such problem & my personal opinion is expressed as follow. I fully agree with views expressed so far. But bag to differ that " Code is a law, with engineering judgments. Hence the inspector has the rights to declare that the original HT was inadequate." Inspectors & total industry must resist the "REJECTION" . We as intellectual & having seniority must become practical. How the code will revise???. ANS.: One is experiments (Pure research) & second is such chances that gives opportunity to experiment !!! _______________________________________________________________________________________________ My understanding is that it is P1 material. In that case every pass normalizes the immediate bottom pass. Hence code requirement for P1 FOR MANDATORY SR is 32 mm & above thickness. SOLUTION:  In any case 0. After SR=PWHT no PTC testing is required as per code--Unless for low temp. vessels. That means code ...