Skip to main content

Re: [MW:31432] Clarification

Thanks,

According to our specification for stainless steel not required an Impact test.
But MDMT is -196°C so Shall I required an Impact test.
Please advise me what are the parameter shall i include in WPS.
Regards
Kiran


On Fri, Sep 11, 2020 at 1:48 PM ahmmad ali mohammed <ali47.alisha@gmail.com> wrote:
Dear mr.Karan, 
Can u please confirm the service design temperature or any impact test done during PQR if done confirm the test temperature.


Sent from my iPhone

On 11 Sep 2020, at 11:53 AM, Vishwas Keskar <vvkeskar123@gmail.com> wrote:


Dear Kiran, 

The query is tricky one. Bt pl note that you have qualified PQR wIth Flux cored welding wire for root pass and then filler with Solid  filler wire .

Refer QW404.23 , Filler metal Product form is essential . Though you are not using that flux cored  filler for root pass  and want to use ER 308L Solid wire with backing gas  , ASME SEC IX  is not that clear to address this  query straightforward.

<image.png>


Advise - Qualify new PQR 

On Fri, Sep 11, 2020 at 9:44 AM Kiran Ekbote <karan.hbl@gmail.com> wrote:
Dear Vishwas /  George,

Please I need more clarification on my above query.
Can I use the second process or not, if not please clarify my doubt with code reference.
And if yes also, please update me, what are the parameter shall I mention in WPS.

And thanks for your response.

Regards
Kiran

On Thu, Sep 10, 2020 at 6:19 PM Vishwas Keskar <vvkeskar123@gmail.com> wrote:
it seems that 
You do not want  to use ROOT PASSS WITH FLUX CORED filler wire and want to use solid wire with backing gas.

The  query is tricky one.
it has many variables 

Joint design :Welding with backing  to  Welding without backing
Backing gas :Addition of backing gas with Solid  filler wire

Qw 404.23  and QW 402.5 are there but not that clear to support your  query.

Advice :Qualify PQR with backing gas with Solid Wire ER308L for root pass as well as filler passes.




On Thu, 10 Sep 2020, 12:19 K K, <karan.hbl@gmail.com> wrote:

Dear All, 

Please clarify some below points. 

I have previously qualified PQR, details as below.

PQR with ASME sec.IX and B31.3 and API 582.  

Process - GTAW (Manual)

Base Metals - ASTM A312 TP304L to STM A312 TP304L

P.No - P8 Gr.1 to P8 Gr.1 

Test coupon Thickness - 5.54 mm

First Process - GTAW - SFA - 5.22,  AWS - R308LT1-5 , F.No - 6, 

A.No - 8, Size of Filler .M - 2.2 , F.M.Product from - Flux-cored, Weld Metal Thickness - 

1.5mm.

Second Process - GTAW - SFA - 5.9,  AWS - ER308L , F.No - 6, 

A.No - 8, Size of Filler .M - 2.5 , F.M.Product from - Solid, Weld Metal Thickness - 

4.04 mm. 

According to red highlighted (Second process) can I use to prepare WPS.

And Thickness range 1.5 mm to 8.08 mm, other all parameters in WPS shall be as above in red highlighted. 

I don't want to use the first process.

Please let me clarify, if any changes, please guide me to prepare WPS.

Regards

KK





--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f927bb52-b5f0-484b-b5aa-f67b70287c1an%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3NgQje8j-NKd4uH77OY0tsM4i3TZVeYLJedrCWO1UZE0Q%40mail.gmail.com.


--

KIRAN

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMFjUk4%3DAkz-1CLQT6aJ9CTxULAZaUV7qwkEUwjKibc%2BHVZz0Q%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3OKVDGtsrksnzXTz%3DfACfWYQp3dt8T1yFKZiPr9Ba-07A%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/BEEA378D-C3A8-4102-B8A8-037197E72B46%40gmail.com.


--

KIRAN

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMFjUk6jWHDdYsKVUuJPBtzo4sJ%3DLD8QdiuuoMokmao%3Dg4Rj%2Bg%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Re: [MW:14950] RE: 14919] Stress relieving Rejected for 5 min less soaking time.

Dear All, I have been a CONSULTANT FOR such problem & my personal opinion is expressed as follow. I fully agree with views expressed so far. But bag to differ that " Code is a law, with engineering judgments. Hence the inspector has the rights to declare that the original HT was inadequate." Inspectors & total industry must resist the "REJECTION" . We as intellectual & having seniority must become practical. How the code will revise???. ANS.: One is experiments (Pure research) & second is such chances that gives opportunity to experiment !!! _______________________________________________________________________________________________ My understanding is that it is P1 material. In that case every pass normalizes the immediate bottom pass. Hence code requirement for P1 FOR MANDATORY SR is 32 mm & above thickness. SOLUTION:  In any case 0. After SR=PWHT no PTC testing is required as per code--Unless for low temp. vessels. That means code ...