You have to understand that PED requires to perform the tests requires by the relevant harmonized standards. PED does not require to perform the tests as per the Harmonized standards. Also the range of approval has not to be as per the harmonized standards. So if you have a PQR as per ASME IX you perform additionaly impact test, PT and macro and you are done

Στις Δευ, 7 Σεπ 2020, 06:44 ο χρήστης Rajavarman <peraiyur.varman@gmail.com> έγραψε:

As per my experience, PED and EN shall be qualified separately.

They will not consider ASME qualifications and test results.

 

I have done All as per EN standard for previous project.

 

Expert shall correct my answer also.

 

 

என்றும் அன்புடன்,

Best regards,

RAJAVARMAN SELVARAJ

+971561895584

 

From: Vivek Pandey
Sent: Sunday, September 6, 2020 9:24 AM
To: materials-welding@googlegroups.com
Cc: pgoswami
Subject: [MW:31394] Regarding welding qualification ASME Section IX v/s EN15614-1.

 

Dear Sir,

 

I have some queries  regarding welding qualification of ASME &EN Code. 

 

Following queries as mentioned below:

1) can we use qualified  WPQR  as per ASME IXwith additional test as required in BS EN ISO 15614-1-2017+A12019 for design code PED.

 

2) How to decide the level 1 or 2 for welding as per BS EN ISO 15614-1-2017+A12019

 

3) Is it essential to mention both the test methods that is ASME & EN in lab test report?

 

4) welder qualification test carried out as per EN ISO 9606 -2019  under TPI. should required to qualify the same by notified body or can we use the same as per PED code 2014/68/EU annex I para 3.1.2.

 

We have already qualified WPS & PQR as per ASME Sec.IX with supplementary testing of Micro, Hardness, Impact & LPT. Can we use the same for PED.

 

 

 

Awaiting for your reply.

 

Thanks & Regards

Vivek

 

 

 

 

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANCwoYnqFy0zXg9LDy1BxvgJ52Kc%2Bd2ke9Oj5THNQcjraaxvPQ%40mail.gmail.com.

 


Virus-free. www.avast.com

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/5f54d3ad.1c69fb81.64613.6c14%40mx.google.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40CC8bPGar6dWhj%3DpfZCab2BbrDt9Z0Nn6O8k6o35DcQjg%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...