Re: [MW:30697] Procedure qualification

Dear venkatramulu,
What is your construction code & qualification code.
As per asme sec-ix .
The WPS Thickness should be 1.5mm to 50mm


Regards
Sangram

On Mon, Apr 6, 2020 at 13:05, Charles Jacob
<charlesvj@gmail.com> wrote:
Hi dear,  are you using b31.3 as the construction code. 

Pl clarify, 

Regards, 

Charles  V Jacob 
 

On Mon, Apr 6, 2020, 2:00 PM chiluka venkatramulu <ramuluchiluka@gmail.com> wrote:
Dear All,
A welding procedure is qualified with multiple PQRs as below
  1. 3.05mm
  2. 4.19mm
  3. 6.0mm
  4. 25.0mm
With impact requirement.
Now what is the thickness range qualified.

Thanks and regards,
Venkatramulu CH

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAF98%2BdFJX%2B%2B8s4ZU0fCuGeWcGfih9rH_D7EUxJv4hZjPohLgvg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKpzM4Bx4U0Eqy3o1PvdSd7u2H_NazQLHxcrSO4Dy4msO1CNUw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/933621498.1251079.1586171937284%40mail.yahoo.com.

No comments:

[MW:35614] Re: SS FILLER

dear , pl check A number and Gas composition use for ss cant be sutibale same % for duplex., u need to qualified with aditional testing of f...