Re: [MW:30697] Procedure qualification

Ref ASME Sec 9, Ref QW 403.6. since Ur maximum thickness is 6mm, qualified is 1/2T. 

On Mon, 6 Apr 2020 3:30 pm chiluka venkatramulu, <ramuluchiluka@gmail.com> wrote:
Dear All,
A welding procedure is qualified with multiple PQRs as below
  1. 3.05mm
  2. 4.19mm
  3. 6.0mm
  4. 25.0mm
With impact requirement.
Now what is the thickness range qualified.

Thanks and regards,
Venkatramulu CH

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAF98%2BdFJX%2B%2B8s4ZU0fCuGeWcGfih9rH_D7EUxJv4hZjPohLgvg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eN_pNeRpj8hV4Yc4fR3wSWYCY3KdKxxdy-6SkM_WyA-wQ%40mail.gmail.com.

No comments:

[MW:35597] INCONEL 825

Dear all  INCONEL 825 matching filler   ER NI FECR-1 its correct please guide me Regarding  Elavarasan -- https://materials-weldin...