Thursday, April 2, 2020

[MW:30684] Re: Production test coupon

pl. check UG-84-(i)(2)

On Saturday, March 28, 2020 at 12:32:03 PM UTC+5:30, Sachin Dhiman wrote:
Dear experts
 I want to know about PTC in detail , when it's required, what's the relation b/w impact exemption and PTC

Thanks in Advance

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4a8668c1-7f3b-4917-938e-26c79d4b394f%40googlegroups.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...