Re: Re: [MW:29171] Impact test for SA-351 CF8M

SA 351 covers only ASS, Duplex and others in SA352. 

On Thu, 28 Feb 2019 8:49 am muneebslsa@gmail.com, <muneebslsa@gmail.com> wrote:
No, i mean that low temp covers only in SA-352 right? i am in doubt that your CF8M is incompatible for your specific requirement.

Thanks.

Regards,
MOHAMED MUNEEB MAHABOOB

Date: 2019-02-27 21:40
Subject: Re: Re: [MW:29165] Impact test for SA-351 CF8M
Not covered

On Wed, 27 Feb 2019, 6:12 pm muneebslsa@gmail.com, <muneebslsa@gmail.com> wrote:
Is that not a coverage from SA-352?


Regards,
MOHAMED MUNEEB MAHABOOB

 
Date: 2019-02-27 12:52
Subject: Re: [MW:29160] Impact test for SA-351 CF8M
lateral expansion

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Wed, Feb 27, 2019 at 11:52 AM chiluka venkatramulu <ramuluchiluka@gmail.com> wrote:
Dear All,,
We have impact test requirement at -196Deg C for SA351 CF8M.  In this case, shall we need to required both energy observed and lateral expansion?. Please advise.


Regards,
Venkatramulu CH

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...