Re: Re: [MW:29110] PWHT requirements SA350 LF 2 Cl.1

Yes, you do not required a heat treatment as per process or power but as said check line class / PMS, moreover if you are in SA projects exemptions of code requirements are not entertained as SA plays the role of ''the most strignent'' and also check with preheat requirements of notes 3A and 3B as per -W-01X, regardless of 25mm.

Thanks.


Regards,
MOHAMED MUNEEB MAHABOOB
''If you know any art by any means then 
SCULPT IT - no matter how cheap or 
useless it is - JUST SCULPT IT
you will never know when experts will
 be on demand'' 
 
Date: 2019-02-12 15:04
Subject: Re: [MW:29091] PWHT requirements SA350 LF 2 Cl.1
Dear mohanraj 
SA350 LF2 CL1 belongs to P1 
As per b31.3 no need pwht for P1 for 18 mm. Thick . But check with your line class service.
Regards 
Sangram
Welding inspector 

Sent from my iPhone

On 12-Feb-2019, at 10:25 AM, Mohan <ggnanamalli@gmail.com> wrote:

Dear Experts,

Whether PWHT is applicable or not for the material SA350 LF 2 Cl.1 Thickness 18mm.

Regards
G Mohanraj

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...