Wednesday, February 27, 2019

Re: [MW:29158] calculation of strain for cold bend

Hi,
Please find below formula.

Inline image



Thanks& Regards,

 

(Karthik)

Karthikeyan.S

QA/QC Manager
Agon Pacific Co.,Ltd.
M: +66-655-174-397, +66-892-512-282

E-mail : karthik6684@yahoo.com



On ‎Wednesday‎, ‎February‎ ‎27‎, ‎2019‎ ‎09‎:‎20‎:‎30‎ ‎AM‎ ‎+07, asgharialigl@gmail.com <asgharialigl@gmail.com> wrote:



Dear All.

Does anybody have excel sheet or calculation sheet that explain how calculate strain of cold bend based on dia. and radius of bend or angle?

Regards

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...