Got details are as.


1 ) Structural welding needs higher weld deposition rates.

2) Higher Cost of welding considering deposition / consumables / timeframes / applications.

3) Quality demands vs Operations ( If we has product like bridge welding with GTAW, Something to additional / realistic requirements ? )

4) GTAW welding preferred over Piping jobs with looks of aesthetics.

5) Higher dilution & heat inputs.


Thanks & Regards

DINESH VITTHAL SOMWANSHI


असो द्यावी दया तुमच्या लागतसे पाया.

*Pray for others, sometime, You might never need to pray for yourself
again.....*



On Tue, Feb 19, 2019 at 4:44 PM Rajesh NBHH <qualitynbhh@gmail.com> wrote:


Expensive  and slow 


Best Regards, 
Rajesh Nayak 
NBHH ( Inter Steel Factory,UAQ)
PO Box No.-7529
Mobile -055 5954750


On Tue, Feb 19, 2019 at 2:48 PM Dinesh Somwanshi <som.din@gmail.com> wrote:
Dear sir,

Looking for advice why TIG welding not using for structural welding generally.

Please advice ahead.

Thanks & Regards

DINESH VITTHAL SOMWANSHI

BACHELOR IN MECHANICAL ENGINEER


Skype = dinesh somwanshi

असो द्यावी दया तुमच्या लागतसे पाया.

*Pray for others, sometime, You might never need to pray for yourself
again.....*

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...