Re: [MW:29124] Re: Feasibility of Ductile iron A536 Gr65-45-12 with ss316

ENiFe-Ci

On Tue, 19 Feb 2019 10:36 am sandeep kumar <sandeepdhiman63@gmail.com wrote:
weld using ENiCrFe-3.

Regards
Sandeep Kumar

On Tuesday, February 19, 2019 at 5:21:32 AM UTC+3, vivekanandan Sivakumar wrote:
Experts,

I would like to weld the Ductile iron casting to SS316 bolt. Kindly provide your valuable opinions.


Vivekanandan.S

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...