These are structural steels but with impact test requirements. You probably know what J and K stand for or R etc. So You can consider them as P-No.1 materials but with higher grades like 335, you have CS in heat treated delivery conditions (N/Q/NT/QT etc) so they may have different group numbers.

Please note that you should not expect to find exact equivalent but there are grades which are practically the same. You may refer ASTM document DS67 for comparing different Steel standards. but again, you may not find the exact equivalent. 

European classification is more precise for structural steels. ASME is not "known" as detailed as Euro-norms when it comes to structural steels. Of course, P-No./Gr-No. classification in ASME is still reliable and useful but my recommendation is not insisting on finding an equivalent grade for your material further than P-No/Gr-No. You can see this with J or K grades which are not well-distinguished in ASME, not mentioning impact test temperature requirements or weather resistant grades.   

Regards
Ramin  Kondori
Sr. QA/QC & Welding Engineer
-----------------------------------------------------------
PG-Dip. in Welding Engineering (IWE  AT  0070)
BSc. in Civil Engineering (IUT)
BGAS Painting Inspector
ASNT Level I&II
                        
IIW-Logo-Colour-small


On Mon, Feb 18, 2019 at 2:52 PM Rajesh <qualitynbhh@gmail.com> wrote:
As per AWS D1.1 unlisted material subjected to New WPS  i agree.
but if 275JR to 275JR wps can we  considered to other grades those material impact properties  are not effecting (temp  )
 Can we consider   these are  single Group (235JR,,275JR,355JR) and weld wrto 275JR approved WPS.


On Thursday, May 7, 2015 at 9:39:17 AM UTC+4, aru ara wrote:
Dear,

you cannot get exact equivalent.

But nearby grade is ASTM A36   

ELAVARASAN ARUMUGAM
Mechanical Engineer 
 

On Wed, May 6, 2015 at 9:45 AM, R R Menon <ranjith....@gmail.com> wrote:
Hiii

its equivalent to ASTM A529

On Saturday, 23 July 2011 15:16:35 UTC+3, PRAMODH NAIR wrote:
Experts,
 
Could you please give me the equivalent ASTM material for EN S275JR with reference code document.
 
Regards
Pramodh

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/394a3b77-8a49-4504-8a9f-4c150b4ba3d8%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...