Saturday, February 16, 2019

Re: [MW:29115] PWHT requirements SA350 LF 2 Cl.1

Dear Mohan:

You did not mention your service requirements, that information is required to answer your question but I guess that it is cold temperature service.

in general, since these grades have impact toughness requirements, My recommendation is yes, go for PWHT otherwise your HAZ impact specimens may fail.

Regards
Ramin  Kondori
Sr. QA/QC & Welding Engineer
-----------------------------------------------------------
PG-Dip. in Welding Engineering (IWE  AT  0070)
BSc. in Civil Engineering (IUT)
BGAS Painting Inspector
ASNT Level I&II
                        
IIW-Logo-Colour-small


On Tue, Feb 12, 2019 at 10:56 AM Mohan <ggnanamalli@gmail.com> wrote:
Dear Experts,

Whether PWHT is applicable or not for the material SA350 LF 2 Cl.1 Thickness 18mm.

Regards
G Mohanraj

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...