Re: [MW:29102] Re: Regarding orientation of specimen

pl ref SA 20
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Wed, Feb 13, 2019 at 11:11 AM sandeep kumar <sandeepdhiman63@gmail.com> wrote:
In rolled steel the grain orientation are parallel to the rolling direction and this help for improved mechanical properties in the rolling direction in contrast to the transverse to rolling direction. A specimen orientation perpendicular to the rolling direction will ensure that material is able to offer the minimum specified properties in the worst scenario. This clause doesn't apply to the casting or forging material.

Considering the XYZ axis of plate where X is the rolling direction or length, Y is the plate width and Z is the thickness. The mechanical properties are degraded in decrements order of X-Y-Z where Z will have the lowest values.

Thanks & regards
Sandeep Kumar


On Thursday, February 7, 2019 at 5:24:28 AM UTC+3, Souravbohray wrote:
I did it from Google also but I didn't understand?
I opened ASME sec 2 part A and sa370 I observed orientation of specimen for testing.i got we have to select orientation of specimen as per code but my question y mostly spec says long axis of specimen should be perpendicular to direction of rolling if we take parrel than what will be effect?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...