Tuesday, February 12, 2019

Re: [MW:29091] PWHT requirements SA350 LF 2 Cl.1

Dear mohanraj 
SA350 LF2 CL1 belongs to P1 
As per b31.3 no need pwht for P1 for 18 mm. Thick . But check with your line class service.
Regards 
Sangram
Welding inspector 

Sent from my iPhone

On 12-Feb-2019, at 10:25 AM, Mohan <ggnanamalli@gmail.com> wrote:

Dear Experts,

Whether PWHT is applicable or not for the material SA350 LF 2 Cl.1 Thickness 18mm.

Regards
G Mohanraj

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...