Re: [MW:29091] grain size requirements for 321H stainless steel

Hi Ramin

Please note, my question is what does mean the coarse?
a higher ASTM no or smaller no.

Thanks.

On Monday, February 11, 2019 at 5:24:06 AM UTC+3, Ramin Kondori wrote:
This number is related to the Number of grains in an specific area.
higher number of grains means they are smaller grains or fine grain.


Ramin  Kondori
Sr. QA/QC & Welding Engineer
-----------------------------------------------------------
PG-Dip. in Welding Engineering (IWE  AT  0070)
BSc. in Civil Engineering (IUT)
BGAS Painting Inspector
ASNT Level I&II
                        
IIW-Logo-Colour-small


On Sun, Feb 10, 2019 at 2:22 PM sandeep kumar <sandeep...@gmail.com> wrote:
Dear all

Please advise your views on below query:

ASTM A182 10.1.2 Grades F 321H, F 347H, and F 348H shall have a
grain size of ASTM No. 7 or coarser.


What does it stand for coarser? 
Does it mean a higher ASTM grain size no (e.g. 8, 9 and so on) or lower ASTM grain size no. (e.g. 6, 5, 4 and so on)?


Thanks & regards
Sandeep 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...